Calcined kaolin KD-42

Kaolin of this type is obtained by high-temperature processing of raw kaolin (at 1000-1150 °C)
w/w % of iron oxide Fe2O3 not more than
w/w % of aluminium oxide Al2O3 not less than
loss on ignition (LOI) not more than, %
moisture content not more than, %
1,5
42
2
1
scores